Crucial checking issues of stainless steel wire mesh?
 

Wire Diameter

Mesh No. per inch

Size (roll or panel size)

Surface condition: opening, color, flat or not and defects.
 

Edge of wire mesh should be neat and without defects.

 

Standard of Checking reed?
The steel reed should be flat and clean, with correct wire going, the inside height, inside length and thickness should be correct.

 

What are the common wire mesh defects?

 

 

1. Folding Marks: The stripe marks on wire mesh surface that cannot be erased.
   
2. Broken Holes:
Multi-pieces broken wires at same site to form a hole in the surface.
 
3. Rusty Spots:
Colored changed by corrosion. Color spots in the surface.
   
4. Broken Wire:
Broken of single wire.
   
5. Wire Back:
The wire coiled, tied or twisted into the mesh forms a protruding above surface. Weft wire tied up called dead coiling. These will mostly cause the opening exceeding maximum opening range, or the wire mesh surface protruding.
   
6. Knot Bulging:
Warp wire not well knotted causes bulging out of the surface.
   
7. Weft Twisting:
Weft wire twists.
   
8. Wire Doubling:
Two pieces of wire or more get into one. Where there should be only one weft or warp wire, inserted two or more wires.
   
9. Mistaken Weaving:
Some weft wire or warp wire are woven together in error. Easily happen for diamond wire mesh.
   
10. Loosening of Wire:
Twisting or moving of single or some pieces of warp wire or weft wire.
   
11. Weaving In of Impurity:
Non-woven materials woven in the fabric cause deformed opening or blocking to affect the neatness of surface. The soft stuff that cannot be moved, also not protruding, may remain as defects; the hard and protruding stuff must be picked out, otherwise it may damage the neighboring wire mesh.
   
12. Flattened Wire: Weft or warp wire deformed by mechanical operation may cause deformed opening when woven into wire mesh.
13. Density Error: Aperture density exceeding density scope causes unqualified mathematics average value of aperture.
14. Weft Wire Backward: Weft wire backward may cause irregular aperture or even worse, to make the opening exceeding deviation allowance.
15. Irregular Aperture: Regular big or small openings between weft wires. One big opening is followed with one small opening for Plain Woven wire mesh. For Twill Woven, usually two big opening then two small, or one big then three small, etc.
16. Bulging Out: One site or some sites along warp direction bulges out, while the aperture does not change much. This kind of defect influences the surface quality of wire mesh.
17. Cloud Shape Weaving: Cloud shape bulging formed in the surface of wire mesh. Caused by weft wire pressed in a different direction. Usually occurs during weaving of medium sized wire mesh.
18. Roll loosening: The wire mesh has no intensive feeling, can be twisted along warp or weft wire at an angle of 45°.
19. Other defects: Including dirty surface, mechanical folding, rusty spots, extra roll width difference, insufficient roll length, breaking of wire mesh, etc.

 

About Qinghe
Company History
About The Name
Meet The Sales
Mission, Vision &Values
Business Culture
Testimonials
Our Brands
Why Qinghe
How To Judge A Company
ISO 9000
Why No Price List
Inquiry Tips
Payment Terms
Sample Policy
M.O.Q
Lead Time
Contact Us
How To Visit Us
Want Us To Visit You